3M EC-2815

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-2815

Main features

  • Flame Retardant Interior Bonding
  • Controlled Honeycomb Insert Placement
  • Extended Aerospace Assembly Window

Product Description

3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a white, flame-retardant two-part epoxy for metal and composite honeycomb structures, insert bonding, and aircraft-interior panels. Mix Part B and Part A at 100:50 by volume; the thixotropic paste resists sagging and provides more than 60 minutes of work life at 22 deg C. Full cure is achieved in 24 hours at 24 deg C or one hour at 82 deg C. The cured adhesive reaches 5000 psi aluminum overlap shear and meets the stated 14 CFR 25.853(a) flammability requirements before and after environmental conditioning.

Key features

  • Flame Retardant Interior Bonding: The cured adhesive meets the stated 14 CFR 25.853(a) flammability requirements.
  • Non Sag Honeycomb Placement: Thixotropic paste controls application in panels, inserts, and vertical joints.
  • Extended Assembly Work Life: More than 60 minutes supports dispensing, positioning, and fixture setup.

Applications

Aircraft-interior honeycomb panels, insert bonding, galleys, luggage bins, partitions, lavatories, seating structures, and sidewall panels.

Product Family

3M EC-2815

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two (Amine / Epoxy)
Other Properties
Storage TemperatureStorage Temperature
7- 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorWhite-Before mixing
Part A colorGray-Before mixing
Mix ratio by weight100:40B:ATwo-part system
Mix ratio by volume100:50B:ATwo-part system
Solids100%Both components
ConsistencyThixotropic paste-Mixed adhesive
Work lifeMore than 60minAt 22 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorWhite-Cured
Density1.3g/cm3Cured; typical
Volatile loss on cureLess than 0.1%Cured adhesive
Overlap shear strength5000psiAluminum; ASTM D1002; tested at 24 deg C
Floating roller peel strength33piwAluminum with EW-5000 primer; ASTM D3167 at 24 deg C
Tensile strength8200psiASTM D638; controlled heat cure
Elongation at break3.4%ASTM D638; controlled heat cure

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers