Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M DP605NS

Main features

  • Tough Flexible Urethane Bond
  • Five Minute Assembly Work Life
  • Non Sag Placement Control

Product Description

3M Scotch-Weld Urethane Adhesive DP605NS, Off-White is a two-part, non-sag urethane adhesive that forms tough, flexible bonds on prepared wood, selected plastics, painted metals, ceramics, and glass. The 1:1 mix ratio and 5 minute work life support fast assembly, while the thixotropic consistency controls placement on vertical or contoured joints. Handling strength develops in 15 to 20 minutes at 23 deg C. The cured off-white adhesive combines 100% elongation with peel and overlap-shear performance for assemblies that require flexibility.

Key features

  • Tough Flexible Urethane Bond: The cured adhesive combines structural attachment with 100% elongation.
  • Five Minute Assembly Work Life: The fast work life supports rapid placement and fixturing.
  • Non Sag Placement Control: Thixotropic consistency resists running on vertical and contoured joints.

Applications

Bonding prepared wood, selected plastics, painted metals, ceramics, glass, and flexible industrial assemblies.

Product Family

3M DP605NS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Off-White
Component SystemComponent System
Two
Other Properties
Storage TemperatureStorage Temperature
15 - 27 °C
Electrical Properties
Volume ResistivityVolume Resistivity
1.0 x 10¹⁴ Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
41 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorWhite-Before mixing
Part A colorTan-Before mixing
Mix ratio by volume1:1B:ATwo-part system
Mix ratio by weight1:1B:ATwo-part system
Part B density8.8 to 9.2lb/galAs supplied
Part A density9.7 to 10.2lb/galAs supplied
Work life5min10 g mass, 1/4 in thick at 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorOff white-Cured
Hardness60 to 65Shore DASTM D2240
Elongation100%ASTM D882 basis
Glass transition temperature41deg CDSC, second heat
Overlap shear on aluminum650psiASTM D1002 at 23 deg C; MEK, abrade, MEK preparation
Floating roller peel on aluminum33piwASTM D3167 at 23 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers