3M 9672

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 9672

Main features

  • High Tack Transfer Bonding
  • Heavy Liner Converting Support
  • Broad Substrate Peel Performance

Product Description

3M Adhesive Transfer Tape 9672 uses fibered Adhesive 300 on a robust polycoated kraft release liner for converting and pressure-sensitive attachment. The 5 mil tape construction supports thin bonding for graphic overlays, metal nameplates, rating plates, and foam laminations. Firm application pressure builds initial contact, and adhesion continues to develop after assembly. Qualified peel data covers ABS, polypropylene, and stainless steel under controlled conditions. The heavier liner improves handling during die cutting and placement while protecting the adhesive until the part is ready for bonding.

Key features

  • Fibered Acrylic Adhesive: Adhesive 300 provides high tack for pressure-sensitive attachment.
  • Heavy Polycoated Liner: The 83 lb kraft liner supports converting and part handling.
  • Broad Substrate Adhesion: Qualified peel data covers ABS, polypropylene, and stainless steel surfaces.

Applications

Graphic overlays, metal nameplates, rating plates, and foam lamination for gasket fabrication.

Product Family

3M 9672

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Tan with green 3M print
Total ThicknessTotal Thickness
130 μm
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Adhesive typeFibered acrylic Adhesive 300-As supplied
Total tape thickness5milNominal
Release liner83 lb polycoated kraft-Tan with green print
Liner thickness6.2milNominal
ColorTan-Liner appearance
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Peel adhesion on ABS4.4N/cm90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min
Peel adhesion on polypropylene6.8N/cm90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min
Peel adhesion on stainless steel9.4N/cm90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min
Short-duration temperature resistance121deg CMinutes to hours
Long-duration temperature resistance70deg CDays to weeks

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers