3M 9472
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- High Tack Transfer Bonding
- Converter Friendly Fiber Reinforcement
- Broad Substrate Peel Performance
Product Description
3M Adhesive Transfer Tape 9472 uses fibered Adhesive 300 on a tan densified kraft release liner to support thin, high-tack attachment. The 5 mil tape construction provides conformability for graphic overlays, metal nameplates, rating plates, and foam lamination. Pressure-sensitive bonding develops with firm application pressure, while adhesion continues to build after assembly. Performance data covers common substrates including ABS, polypropylene, and stainless steel under controlled peel conditions. The liner protects the adhesive during converting and can support die-cut parts before final placement.
Key features
- Fibered Acrylic Adhesive: Adhesive 300 combines high tack with handling support for converting.
- Five Mil Tape Construction: The thin adhesive layer supports overlays, nameplates, and foam laminations.
- Broad Substrate Adhesion: Qualified peel data covers ABS, polypropylene, and stainless steel surfaces.
Applications
Graphic overlays, metal nameplates, rating plates, and foam lamination for gasket fabrication.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive type | Fibered acrylic Adhesive 300 | - | As supplied |
| Total tape thickness | 5 | mil | Nominal |
| Release liner | 60 lb densified kraft | - | Tan liner |
| Liner thickness | 3.5 | mil | Nominal |
| Color | Tan | - | Liner appearance |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Peel adhesion on ABS | 4.4 | N/cm | 90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min |
| Peel adhesion on polypropylene | 6.8 | N/cm | 90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min |
| Peel adhesion on stainless steel | 9.4 | N/cm | 90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min |
| Short-duration temperature resistance | 121 | deg C | Minutes to hours |
| Long-duration temperature resistance | 70 | deg C | Days to weeks |