3M 79
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Stable Glass-Cloth Coil Insulation
- 600 V Electrical Tape Rating
- High-Temperature Motor and Transformer Use
Product Description
3M Glass Cloth Electrical Tape 79 is a white 7 mil electrical tape with a 5 mil glass-cloth backing and non-corrosive acrylic pressure-sensitive adhesive for coil, transformer, and motor insulation work. The glass cloth provides dimensional stability, absorbs varnishes and resins, and remains conformable for banding, anchoring, and crossover insulation. Electrical performance includes a minimum 2000 V dielectric breakdown and minimum 50 x 10^6 ohm insulation resistance under ASTM D1000 testing. The tape is printable, solvent resistant, and rated for 600 V service, with product-page temperature performance from 0 to 150 deg C.
Key features
- Stable glass-cloth backing: The 5 mil glass cloth provides a stable, conformable carrier that absorbs varnishes and resins in coil and motor assemblies.
- Electrical insulation performance: Minimum 2000 V dielectric breakdown and 50 x 10^6 ohm insulation resistance provide measured electrical insulation performance.
- High-temperature electrical use: The tape is rated for 600 V service and withstands 0 to 150 deg C for high-temperature electrical assembly work.
Applications
Use 3M Glass Cloth Electrical Tape 79 for coil covers, banding, core-layer and crossover insulation, lead-pad hold-downs, end turns, lead anchors, and electrical connections in transformers and motors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | White | Visual | |
| Backing | Glass cloth | Product construction | |
| Adhesive | Acrylic pressure-sensitive adhesive | Non-corrosive construction | |
| Backing thickness | 5 | mil | Nominal; 0.127 mm |
| Total thickness | 7.0 +/- 1.0 | mil | ASTM D1000; 0.178 +/- 0.025 mm |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesion to steel | 30 | oz/in | Minimum; ASTM D1000; 3.3 N/cm |
| Dielectric breakdown | 2000 | V | Minimum; ASTM D1000 |
| Insulation resistance | 50 x 10^6 | ohm | Minimum; ASTM D1000 |